Day 2026-01-18 (q3k, rob, hugo, rahix)
first prototype of spincoater hardware:
An unknown quantity of PMMA was added to an unknown quantity of acetone. Solution was refluxed at 50 degrees on a hot plate for ~30 minutes. PMMA was not fully dissolved by time of use.
A micropipette was used to dispense the PMMA/Acetone solution on a test setup without RPM feedback.
Variable space was explored semi-arbitrarily. Spin time was around 10s. Acceleration was controlled by the ESC.